Enhancement of Aqueous Corrosion of Zircaloy-4 Due to Hydride Precipitation at the Metal-Oxide Interface
Enhancement of Aqueous Corrosion of Zircaloy-4 Due to Hydride Precipitation at the Metal-Oxide Interface
- Статус документа:
- D
- Формат:
- Электронный (PDF)
- SKU:
- ASTM STP25527S
Цена по запросу
Свяжитесь с нами для уточнения стоимости.
Abstract
Long-term static autoclave corrosion tests were conducted on Zircaloy-4 tube specimens in water at 633 K. The material variables included in this investigation were: annealing parameter range 10-17 to 10-19 h (with Q/R = 40 000 K). fabricat...