Найдено: 6
Overview ISO 12884:2000 specifies a validated procedure for measuring total polycyclic aromatic hydrocarbons (PAH) in ambient air by collecting both gas-phase and particle-phase PAH on a combined fin…
Overview ISO 1288-5:2016 (Glass in building - Determination of the bending strength of glass - Part 5) specifies the coaxial double‑ring test for measuring the comparative bending strength of flat gl…
Overview ISO 1288-1:2016 - "Glass in building - Determination of the bending strength of glass - Part 1: Fundamentals of testing glass" defines the fundamental principles for measuring the bending st…
Overview ISO 1288-4:2016 - Glass in building - Determination of the bending strength of glass - Part 4: Testing of channel shaped glass specifies a laboratory method to determine the profile bending…
Overview ISO 1288-3:2016 - Glass in building - Determination of the bending strength of glass - Part 3: Test with specimen supported at two points (four point bending) specifies a laboratory method t…
Overview ISO 1288-2:2016 - Glass in building: Coaxial double-ring test on flat specimens with large test surface areas specifies a standardized laboratory method to determine the bending strength of…